FINE - GRAIN PROCESSING
The grain we see in grainy photographs is not the individual particles or grains of silver which make up the negative image . Those individual particles are much too small for that , even when the negative is enlarged to photo - mural size . What we see as grain is the pattern obtained through the grouping or clumping together of large numbers of individual particles into random arrangements , which then become visible as grain .
This clumping action takes place during the processing of the negative ; by far the greater part of it during development . Anything which facilitates or promotes this clumping action increases grain . Let us list some of the more important causes .
THE TYPE OF FILM . Actually , this is the most important factor in determining grain size . You can reduce the grain size of a coarse - grained film through proper processing techniques , but it will still be grainier than a finer - grained film which has received ordinary handling . Generally speaking , the fast films show considerably more clumping action and , therefore , coarser grain than do the slow films . This is largely because crystals of silver bromide in the emulsion of fast films are relatively large , and larger crystals clump together on being developed more readily than smaller crystals . For fine - grain results , therefore , avoid the fastest films .
PROLONGED PROCESSING TIME . When gelatin becomes wet , it absorbs water and swells up . The longer it remains wet , the greater is the swelling . Clumping proceeds at a higher rate when the gelatin is highly swollen . Swelling action of gelatin is greatest in alkaline solutions , and developers are alkaline .
OVERDEVELOPMENT . In the process of development , a certain amount of internal chemical agitation of the silver particles occurs as they are formed . This internal agitation of the silver results in clumping . Prolonged development beyond that which is necessary to produce a good negative increases such clumping .
OVEREXPOSURE . An overexposed film develops rapidly and to a greater than normal density . Both the rapid development and the greater silver deposit result in greater internal agitation of the emulsion and larger grain .
VIGOROUS , QUICK - ACTING DEVELOPERS . These promote rapid development which results in high internal agitation of the emulsion and , therefore , larger grain . There is an apparent contradiction in the fact that the developers recommended for the slow , thin - emulsion , fine - grain films are generally vigorous developers . This apparent contradiction is explained later .
VARYING TEMPERATURE OF PROCESSING SOLUTIONS . The swelling of wet gelatin increases with temperature . If a film is developed at 72 ° F. , rinsed in cold tap water ( 60 ° F . ) , fixed at an 80 ° room temperature , and washed in cold water ( 60 ° F. ) , the gelatin passes through two cycles of swelling and shrinking . This results in internal motion of the silver image and increases grain .
HIGH TEMPERATURE PROCESSING . The reason here is two - fold . Developer action is more vigorous , and gelatin swells to a greater degree . Both factors increase grain size . However , there are special high temperature developers which contain additives to prevent excessive gelatin swelling , so that grain need not be excessive with proper , high - temperature , processing techniques .
التصوير الفوتوغرافي الحديث
التصوير الفوتوغرافي ٣٥ مم
معالجة الحبوب الدقيقة
معالجة الحبوب الدقيقة
الحبوب التي نراها في الصور المحببة ليست جزيئات الفضة أو حبيباتها التي تشكل الصورة السلبية. هذه الجسيمات الفردية صغيرة جدًا لذلك ، حتى عندما يتم تكبير الصورة السلبية إلى الصورة - الحجم الجداري. ما نراه كحبوب هو النمط الذي تم الحصول عليه من خلال تجميع أو تجميع أعداد كبيرة من الجسيمات الفردية معًا في ترتيبات عشوائية ، والتي تصبح بعد ذلك مرئية كحبوب.
يحدث هذا الإجراء المتكتل أثناء معالجة السلبية ؛ إلى حد بعيد الجزء الأكبر منه أثناء التطوير. أي شيء يسهل أو يعزز هذا التكتل يزيد من الحبوب. دعونا نذكر بعض الأسباب الأكثر أهمية.
نوع الفيلم. في الواقع ، هذا هو العامل الأكثر أهمية في تحديد حجم الحبوب. يمكنك تقليل حجم الحبيبات للفيلم ذي الحبيبات الخشنة من خلال تقنيات المعالجة المناسبة ، لكنه سيظل أكثر تحببًا من الفيلم الحبيبي الدقيق الذي تم التعامل معه بشكل عادي. بشكل عام ، تُظهر الأفلام السريعة حركة أكثر تكتلًا بشكل كبير ، وبالتالي ، فهي أكثر خشونة من الأفلام البطيئة. ويرجع ذلك إلى حد كبير إلى أن بلورات بروميد الفضة في مستحلب الأفلام السريعة كبيرة نسبيًا ، وتتجمع البلورات الأكبر معًا عند تطويرها بسهولة أكبر من البلورات الأصغر. للحصول على نتائج دقيقة للحبيبات ، تجنب أسرع الأفلام.
وقت طويل للتجهيز. عندما يصبح الجيلاتين رطبًا ، يمتص الماء ويتضخم. وكلما طالت فترة البلل ، زاد التورم. يحدث التكتل بمعدل أعلى عندما يكون الجيلاتين منتفخًا للغاية. يكون تأثير الجيلاتين المنتفخ أعظم في المحاليل القلوية ، والمطورون قلويون.
التنمية الزائدة. في عملية التطوير ، يحدث قدر معين من التحريض الكيميائي الداخلي لجزيئات الفضة أثناء تكوينها. هذا التحريض الداخلي للفضة ينتج عنه تكتل. إن التطور المطول الذي يتجاوز ما هو ضروري لإنتاج سلبي جيد يزيد من هذا التكتل.
التعرض المفرط . يتطور الفيلم شديد التعرض للضوء بسرعة وبكثافة أكبر من المعتاد. يؤدي كل من التطور السريع ورواسب الفضة الأكبر إلى زيادة التقليب الداخلي للمستحلب والحبوب الأكبر.
قوي وسريع - مطورون فاعلون. هذه تعزز التطور السريع الذي ينتج عنه تهيج داخلي مرتفع للمستحلب ، وبالتالي الحبوب الكبيرة. هناك تناقض واضح في حقيقة أن المطورين أوصوا بالأفلام البطيئة الرقيقة ذات الحبيبات الدقيقة هم مطورون قويون بشكل عام. سيتم شرح هذا التناقض الظاهر لاحقًا.
درجات حرارة متفاوتة لتجهيز الحلول. يزداد تورم الجيلاتين الرطب مع زيادة درجة الحرارة. إذا تم تطوير فيلم عند 72 درجة فهرنهايت ، وشطفه في ماء الصنبور البارد (60 درجة فهرنهايت) ، وتثبيته عند درجة حرارة الغرفة 80 درجة ، وغسلها في ماء بارد (60 درجة فهرنهايت) ، يمر الجيلاتين خلال دورتين من تورم وانكماش. ينتج عن هذا الحركة الداخلية للصورة الفضية ويزيد التحبب.
معالجة درجة حرارة عالية. والسبب هنا ذو شقين. يكون عمل المطور أكثر قوة ، ويتضخم الجيلاتين بدرجة أكبر. كلا العاملين يزيدان حجم الحبوب. ومع ذلك ، هناك مطورو خاص لدرجة الحرارة المرتفعة تحتوي على مواد مضافة لمنع التورم المفرط للجيلاتين ، بحيث لا تحتاج الحبوب إلى الإفراط في استخدام تقنيات المعالجة المناسبة ذات درجة الحرارة العالية.
التصوير الفوتوغرافي ٣٥ مم
معالجة الحبوب الدقيقة
FINE - GRAIN PROCESSING
The grain we see in grainy photographs is not the individual particles or grains of silver which make up the negative image . Those individual particles are much too small for that , even when the negative is enlarged to photo - mural size . What we see as grain is the pattern obtained through the grouping or clumping together of large numbers of individual particles into random arrangements , which then become visible as grain .
This clumping action takes place during the processing of the negative ; by far the greater part of it during development . Anything which facilitates or promotes this clumping action increases grain . Let us list some of the more important causes .
THE TYPE OF FILM . Actually , this is the most important factor in determining grain size . You can reduce the grain size of a coarse - grained film through proper processing techniques , but it will still be grainier than a finer - grained film which has received ordinary handling . Generally speaking , the fast films show considerably more clumping action and , therefore , coarser grain than do the slow films . This is largely because crystals of silver bromide in the emulsion of fast films are relatively large , and larger crystals clump together on being developed more readily than smaller crystals . For fine - grain results , therefore , avoid the fastest films .
PROLONGED PROCESSING TIME . When gelatin becomes wet , it absorbs water and swells up . The longer it remains wet , the greater is the swelling . Clumping proceeds at a higher rate when the gelatin is highly swollen . Swelling action of gelatin is greatest in alkaline solutions , and developers are alkaline .
OVERDEVELOPMENT . In the process of development , a certain amount of internal chemical agitation of the silver particles occurs as they are formed . This internal agitation of the silver results in clumping . Prolonged development beyond that which is necessary to produce a good negative increases such clumping .
OVEREXPOSURE . An overexposed film develops rapidly and to a greater than normal density . Both the rapid development and the greater silver deposit result in greater internal agitation of the emulsion and larger grain .
VIGOROUS , QUICK - ACTING DEVELOPERS . These promote rapid development which results in high internal agitation of the emulsion and , therefore , larger grain . There is an apparent contradiction in the fact that the developers recommended for the slow , thin - emulsion , fine - grain films are generally vigorous developers . This apparent contradiction is explained later .
VARYING TEMPERATURE OF PROCESSING SOLUTIONS . The swelling of wet gelatin increases with temperature . If a film is developed at 72 ° F. , rinsed in cold tap water ( 60 ° F . ) , fixed at an 80 ° room temperature , and washed in cold water ( 60 ° F. ) , the gelatin passes through two cycles of swelling and shrinking . This results in internal motion of the silver image and increases grain .
HIGH TEMPERATURE PROCESSING . The reason here is two - fold . Developer action is more vigorous , and gelatin swells to a greater degree . Both factors increase grain size . However , there are special high temperature developers which contain additives to prevent excessive gelatin swelling , so that grain need not be excessive with proper , high - temperature , processing techniques .
التصوير الفوتوغرافي الحديث
التصوير الفوتوغرافي ٣٥ مم
معالجة الحبوب الدقيقة
معالجة الحبوب الدقيقة
الحبوب التي نراها في الصور المحببة ليست جزيئات الفضة أو حبيباتها التي تشكل الصورة السلبية. هذه الجسيمات الفردية صغيرة جدًا لذلك ، حتى عندما يتم تكبير الصورة السلبية إلى الصورة - الحجم الجداري. ما نراه كحبوب هو النمط الذي تم الحصول عليه من خلال تجميع أو تجميع أعداد كبيرة من الجسيمات الفردية معًا في ترتيبات عشوائية ، والتي تصبح بعد ذلك مرئية كحبوب.
يحدث هذا الإجراء المتكتل أثناء معالجة السلبية ؛ إلى حد بعيد الجزء الأكبر منه أثناء التطوير. أي شيء يسهل أو يعزز هذا التكتل يزيد من الحبوب. دعونا نذكر بعض الأسباب الأكثر أهمية.
نوع الفيلم. في الواقع ، هذا هو العامل الأكثر أهمية في تحديد حجم الحبوب. يمكنك تقليل حجم الحبيبات للفيلم ذي الحبيبات الخشنة من خلال تقنيات المعالجة المناسبة ، لكنه سيظل أكثر تحببًا من الفيلم الحبيبي الدقيق الذي تم التعامل معه بشكل عادي. بشكل عام ، تُظهر الأفلام السريعة حركة أكثر تكتلًا بشكل كبير ، وبالتالي ، فهي أكثر خشونة من الأفلام البطيئة. ويرجع ذلك إلى حد كبير إلى أن بلورات بروميد الفضة في مستحلب الأفلام السريعة كبيرة نسبيًا ، وتتجمع البلورات الأكبر معًا عند تطويرها بسهولة أكبر من البلورات الأصغر. للحصول على نتائج دقيقة للحبيبات ، تجنب أسرع الأفلام.
وقت طويل للتجهيز. عندما يصبح الجيلاتين رطبًا ، يمتص الماء ويتضخم. وكلما طالت فترة البلل ، زاد التورم. يحدث التكتل بمعدل أعلى عندما يكون الجيلاتين منتفخًا للغاية. يكون تأثير الجيلاتين المنتفخ أعظم في المحاليل القلوية ، والمطورون قلويون.
التنمية الزائدة. في عملية التطوير ، يحدث قدر معين من التحريض الكيميائي الداخلي لجزيئات الفضة أثناء تكوينها. هذا التحريض الداخلي للفضة ينتج عنه تكتل. إن التطور المطول الذي يتجاوز ما هو ضروري لإنتاج سلبي جيد يزيد من هذا التكتل.
التعرض المفرط . يتطور الفيلم شديد التعرض للضوء بسرعة وبكثافة أكبر من المعتاد. يؤدي كل من التطور السريع ورواسب الفضة الأكبر إلى زيادة التقليب الداخلي للمستحلب والحبوب الأكبر.
قوي وسريع - مطورون فاعلون. هذه تعزز التطور السريع الذي ينتج عنه تهيج داخلي مرتفع للمستحلب ، وبالتالي الحبوب الكبيرة. هناك تناقض واضح في حقيقة أن المطورين أوصوا بالأفلام البطيئة الرقيقة ذات الحبيبات الدقيقة هم مطورون قويون بشكل عام. سيتم شرح هذا التناقض الظاهر لاحقًا.
درجات حرارة متفاوتة لتجهيز الحلول. يزداد تورم الجيلاتين الرطب مع زيادة درجة الحرارة. إذا تم تطوير فيلم عند 72 درجة فهرنهايت ، وشطفه في ماء الصنبور البارد (60 درجة فهرنهايت) ، وتثبيته عند درجة حرارة الغرفة 80 درجة ، وغسلها في ماء بارد (60 درجة فهرنهايت) ، يمر الجيلاتين خلال دورتين من تورم وانكماش. ينتج عن هذا الحركة الداخلية للصورة الفضية ويزيد التحبب.
معالجة درجة حرارة عالية. والسبب هنا ذو شقين. يكون عمل المطور أكثر قوة ، ويتضخم الجيلاتين بدرجة أكبر. كلا العاملين يزيدان حجم الحبوب. ومع ذلك ، هناك مطورو خاص لدرجة الحرارة المرتفعة تحتوي على مواد مضافة لمنع التورم المفرط للجيلاتين ، بحيث لا تحتاج الحبوب إلى الإفراط في استخدام تقنيات المعالجة المناسبة ذات درجة الحرارة العالية.